Abstract:
The most common use of reclaimed asphalt pavement (RAP) is in the lower layers of a pavement structure, where it has been proven as a valid substitute for virgin materials. The use of RAP in surface mixes is more limited, since a major concern is that the high-RAP mixes may not perform as well as traditional mixes. To reduce risks or compromised performance, the use of RAP has commonly been controlled by specifications that limit the allowed amount of recycled material in the mixes. However, the ability to include greater quantities of RAP in the surface mix while maintaining a satisfying field performance would result in potential cost savings for the agencies and environmental savings for the public. The main purpose of this research was to produce highly recycled surface mixes capable of performing well in the field, verify the performance-based design procedure, and analyze the results. To produce the mixes, a balanced mix design (BMD) methodology was used and a comparison with traditional mixes, prepared in accordance with the requirements of the Virginia Department of Transportation's volumetric mix design, was performed. Through the BMD procedure, which featured the indirect tensile cracking test for evaluating cracking resistance and the Asphalt Pavement Analyzer (APA) for evaluating rutting resistance, it was possible to obtain a highly recycled mix (45% RAP) capable of achieving a better overall laboratory performance than traditional mixes designed using volumetric constraints while resulting in a reduction in production cost.
Related Concept Videos
Design Example: Managing Concrete Workability
Mixing Concrete
Ready Mixed Concrete
Mixing Time
Design Example: Aggregate Gradation
The grading, or particle-size distribution, of sand is determined using sieve analysis, with standard sizes ranging from 150 μm to 10 mm (ASTM No. 100 sieve to 3⁄8 in. sieve). Sand is...
Water Cement Ratio