Abstract:
The addition of natural fibers used as reinforcement has great appeal in the construction materials industry since natural fibers are cheaper, biodegradable, and easily available. In this work, we analyzed the feasibility of using the fibers of piassava, tucum palm, razor grass, and jute from the Amazon rainforest as reinforcement in mortars, exploiting the mechanical properties of compressive and flexural strength of samples with 1.5%, 3.0%, and 4.5% mass addition of the composite binder (50% Portland cement + 40% metakaolin + 10% fly ash). The mortars were reinforced with untreated (natural) and treated (hot water treatment, hornification, 8% NaOH solution, and hybridization) fibers, submitted to two types of curing (submerged in water, and inflated with CO2 in a pressurized autoclave) for 28 days. Mortars without fibers were used as a reference. For the durability study, the samples were submitted to 20 drying/wetting cycles. The fibers improved the flexural strength of the mortars and prevented the abrupt rupture of the samples, in contrast to the fragile behavior of the reference samples. The autoclave cure increased the compressive strength of the piassava and tucum palm samples with 4.5% of fibers.
Related Concept Videos
Mortar Properties
Fiber Reinforced Concrete
Mortar
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Ferrocement
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...