Elucidating the Feature of Intermediate Water in Hydrated Poly(ω-methoxyalkyl acrylate)s by Molecular Dynamics

An-Tsung Kuo1, Toshiki Sonoda2, Shingo Urata1

  • 1Innovative Technology Laboratories, AGC Inc., Yokohama 221-8755, Japan.

Related Concept Videos

Physical Properties of Carboxylic Acids01:31

Physical Properties of Carboxylic Acids

Carboxylic acids with lower molecular weight exhibit a sharp and unpleasant odor. They also have higher boiling and melting points than analogous compounds, such as aldehydes, ketones, and alcohols.
6.0K
Aldehydes and Ketones with Water: Hydrate Formation01:20

Aldehydes and Ketones with Water: Hydrate Formation

An oxygen-based nucleophile, like water, can undergo addition reactions with aldehydes and ketones. The reaction leads to the formation of hydrates, also referred to as 1,1-diols or geminal diols.
The formation of hydrates is a reversible reaction. Hydrate formation is influenced by steric and electronic factors accompanying the alkyl substituents on the carbonyl group: The rate of hydrate formation increases with a decrease in the number of alkyl groups attached to the carbonyl carbon. Hence,...
4.3K
Regioselectivity and Stereochemistry of Acid-Catalyzed Hydration02:34

Regioselectivity and Stereochemistry of Acid-Catalyzed Hydration

The rate of acid-catalyzed hydration of alkenes depends on the alkene's structure, as the presence of alkyl substituents at the double bond can significantly influence the rate.
9.1K
Acid-Catalyzed Hydration of Alkenes02:45

Acid-Catalyzed Hydration of Alkenes

Alkenes react with water in the presence of an acid to form an alcohol. In the absence of acid, hydration of alkenes does not occur at a significant rate, and the acid is not consumed in the reaction. Therefore, alkene hydration is an acid-catalyzed reaction.
16.3K
Aqueous Solutions and Heats of Hydration02:42

Aqueous Solutions and Heats of Hydration

Water and other polar molecules are attracted to ions. The electrostatic attraction between an ion and a molecule with a dipole is called an ion-dipole attraction. These attractions play an important role in the dissolution of ionic compounds in water.
When ionic compounds dissolve in water, the ions in the solid separate and disperse uniformly throughout the solution because water molecules surround and solvate the ions, reducing the strong electrostatic forces between them. This process...
16.6K