Mechano-responsive hydrogen-bonding array of thermoplastic polyurethane elastomer captures both strength and
Youngho Eom1, Seon-Mi Kim2, Minkyung Lee2
1Department of Polymer Engineering, Pukyong National University, Busan, 48513, Republic of Korea.
Abstract:
Self-repairable materials strive to emulate curable and resilient biological tissue; however, their performance is currently insufficient for commercialization purposes because mending and toughening are mutually exclusive. Herein, we report a carbonate-type thermoplastic polyurethane elastomer that self-heals at 35 °C and exhibits a tensile strength of 43 MPa; this elastomer is as strong as the soles used in footwear. Distinctively, it has abundant carbonyl groups in soft-segments and is fully amorphous with negligible phase separation due to poor hard-segment stacking. It operates in dual mechano-responsive mode through a reversible disorder-to-order transition of its hydrogen-bonding array; it heals when static and toughens when dynamic. In static mode, non-crystalline hard segments promote the dynamic exchange of disordered carbonyl hydrogen-bonds for self-healing. The amorphous phase forms stiff crystals when stretched through a transition that orders inter-chain hydrogen bonding. The phase and strain fully return to the pre-stressed state after release to repeat the healing process.
More Related Videos
11:49Synthesis of Soft Polysiloxane-urea Elastomers for Intraocular Lens Application
Published on: March 8, 2019
12:07Fabricating Degradable Thermoresponsive Hydrogels on Multiple Length Scales via Reactive Extrusion, Microfluidics, Self-assembly, and Electrospinning
Published on: April 16, 2018