Related Experiment Video
Updated: Nov 18, 2025

Grafting Multiwalled Carbon Nanotubes with Polystyrene to Enable Self-Assembly and Anisotropic Patchiness
Published on: April 1, 2018
Influence of Carbon Nanotubes on Phase Composition, Thermal and Post-Heating Behavior of Cementitious Composites
Mohammad R Irshidat1, Nasser Al-Nuaimi1, Mohamed Rabie1
1Center for Advanced Materials (CAM), Qatar University, P.O. Box 2713, Doha, Qatar.
Abstract:
This paper experimentally investigates the influence of carbon nanotubes (CNTs) on phase composition, microstructure deterioration, thermal behavior, and residual mechanical strengths of cementitious composites exposed to elevated temperatures. Cement mortars with small dosages of CNTs, 0.05% and 0.2% by weight of cement, were prepared and then heated at 25 °C, 150 °C, 200 °C, 450 °C, and 600 °C for two hours before being tested. The results show positive impact of the CNTs on the hydration process of cement mortar at room temperature and at higher temperatures up to 200 °C. Decomposition of the hydration products is obvious at 450 °C, whereas sever deterioration in the microstructure occurs at 600 °C. The nano reinforcement and bridging effect of the CNTs are obvious up to 450 °C. Thermal behavior characterization shows that CNTs incorporation enhances the thermal conductivity of the unheated and heat-treated mortar specimens. The decomposition of the hydration products needs more heat in the presence of CNTs. Finally, presence of CNTs significantly enhances the residual compressive and flexural strengths of heated mortar specimens for all studied temperatures.
Related Concept Videos
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
Hydration of Cement
Porosity in Cement Paste
The balance of water to cement in the mix is...
Types of Cement I
Type I (Ordinary Portland Cement) is widely used for general construction where special properties are not required. It has moderate sulfate resistance and heat of hydration.
Type II (Modified Cement) offers moderate resistance to sulfate attack and a lower rate of heat development compared to Type I. It is suitable for structures in...
Setting Time of Cement
Strength of Cement