Effect of Neutralizer on Transparency of Nucleating Agent-Containing Polypropylene
Shohei Iwasaki1,2, Yohei Uchiyama2, Miwa Tenma1
1School of Materials Science, Japan Advanced Institute of Science and Technology, 1-1 Asahidai, Nomi, Ishikawa 923-1292, Japan.
Abstract:
The effects of neutralizer species on the transparency of injection-molded plates were studied using isotactic polypropylene (PP) containing a crystal nucleating agent-i.e., 1,3:2,4-bis-o-(4-methylbenzylidene)-d-sorbitol (MDBS). A plate containing lithium stearate (StLi) was more transparent than one containing calcium stearate (StCa) when the MDBS content was 0.1 wt. %. The addition of StLi accelerated the formation of MDBS fibers and the crystallization of PP. However, when the MDBS content was 1.0 wt. %, StCa improved the transparency more effectively than StLi. These results indicate that the combination of an appropriate amount of MDBS and the correct neutralizer species is critical for enhancing the transparency of injection-molded PP plates.
Related Concept Videos
Polymer Classification: Stereospecificity
Anionic Chain-Growth Polymerization: Overview
Ziegler–Natta Chain-Growth Polymerization: Overview