Effect of Compaction Pressure and Moisture Content on Post-Agglomeration Elastic Springback of Pellets

Jakub Styks1, Adrian Knapczyk1, Bogusława Łapczyńska-Kordon1

  • 1Department of Mechanical Engineering and Agrophysics, University of Agriculture in Krakow, Balicka 120, 31-120 Kraków, Poland.

Related Concept Videos

Moisture Content and Bulking of Aggregate01:10

Moisture Content and Bulking of Aggregate

The moisture content of aggregates is a crucial factor in construction, particularly in concrete mixing, as it influences the total water required in the mix. Moisture content represents the water coated on the exterior surface of the aggregate existing in a saturated and surface-dry condition. The total water content of a moist aggregate is the sum of its moisture content and water absorption.
When aggregates are exposed to rain or sit in stockpiles, they absorb moisture, which must be...
327
Compacting Factor test01:22

Compacting Factor test

The compacting factor test is a method used to assess the workability of concrete. It is  especially suitable for concrete mixes containing aggregates up to one and a half inches in size. This test involves specialized equipment consisting of two truncated cone-shaped hoppers and a cylinder, all with polished interior surfaces to minimize friction.
The procedure begins by placing concrete into the upper hopper without any compaction. Once filled, the bottom door of this hopper is opened,...
382
Plastic Behavior01:21

Plastic Behavior

A material's elastic behavior is characterized by the disappearance of stress once the load is removed, allowing the material to return to its original state. However, when stress surpasses the yield point, yielding commences, marking the onset of plastic deformation or permanent set. This change from elastic to plastic behavior is influenced by the peak stress value and the duration before the load is removed. An intriguing observation occurs when a specimen is loaded, unloaded, and...
369
Unsoundness of Aggregate due to Volume Change01:26

Unsoundness of Aggregate due to Volume Change

Unsoundness in aggregates due to volume changes is primarily caused by the physical alterations aggregates undergo, such as freezing and thawing, thermal changes, and wetting and drying. Unsound aggregates, when subjected to these changes, result in volume change upon disintegration. This, in turn, contributes to the deterioration of concrete, including scaling, pop-outs, and cracking. Particular types of aggregates, such as porous flints, cherts, and those containing clay minerals, are...
263
Porosity and Absorption of Aggregate01:20

Porosity and Absorption of Aggregate

Aggregates contain pores of varying sizes; while some are completely enclosed within the particles, others open onto the surface, allowing water to penetrate. The porosity of aggregates is a major factor contributing to the overall porosity of concrete, given that aggregates constitute about three-quarters of concrete's volume.
When all pores in an aggregate are filled with water, the aggregate is considered saturated and surface-dry. If left in dry air, water will evaporate until the...
568
Bulk Density of Aggregate01:22

Bulk Density of Aggregate

Bulk density refers to the mass of aggregate particles that would fill a unit volume. The concept of bulk density originates from the inability to pack aggregate particles in a manner that completely eliminates void spaces. Hence, the term bulk refers to the volume that encompasses both the aggregates and the voids. This measurement is crucial when aggregates are batched by volume and is used to convert quantities by mass to volume.
Most natural mineral aggregates, like sand and gravel,...
877