Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
A randomized clinical trial of dentin hypersensitivity reduction over one month after a single topical application of
Samar Hatem Abuzinadah1, Abdulrahman Jafar Alhaddad2
1Department of Restorative Dentistry, Faculty of Dentistry, King Abdul-Aziz University, Alehtifalat street, Jeddah, 21589, Saudi Arabia. sabuzinadah1@kau.edu.sa.
Abstract:
Dentinal hypersensitivity (DH) is a condition that causes patient discomfort. To evaluate the clinical efficacy of Gluma, fluoride varnish and Tetric N-Bond self-etch system in relieving DH immediately and over 30 days following a single topical application. The present randomized clinical trial was conducted on 55 patients with an age range 20-49 years. 70 teeth in total were incorporated and randomly assigned to the three groups. Parameters examined were: Tactile, air blast, and cold stimuli. VAS was used to assess tactile stimulus whereas the Schiff Cold Scale for air blast and cold stimuli. DH was evaluated immediately, at two weeks and 1 month follow up. Gluma showed a statistically significant reduction in DH scores over other materials. It was concluded that Gluma have statistically significant results over other materials in relieving DH immediately and over 30 days following a single topical application.Trial Registration: Clinical Trials.gov Identifier: NCT04351412, King Abdulaziz University Protocol Record 129-09-19. Registered 17 April 2020 - Retrospectively registered. http://ClinicalTrials.gov/NCT04351412 .