Purpose:
Xenogeneic bone substitute materials are often used for augmentation of larger bone defects. Purification methods for these materials vary, mainly in terms of temperature. The aim of this study was to determine in vivo how sintering affects quantitative and qualitative bone regeneration of 2 bovine augmentation materials.
Methods:
A total of 56 critical size defects were set at the frontal bone of 14 domestic pigs (4 each) and filled randomly with either bovine, sintered hydroxyapatite (BO), bovine, non-sintered hydroxyapatite (BOS), local autologous bone (AB) or left empty. All defects were additionally covered with a collagen membrane. Specimens were harvested after 4 and 8 weeks and were evaluated histologically and histomorphometrically.
Results:
Histologically new bone could be seen in every group. Significantly highest new bone formation was found in AB. No significant difference could be detected between BO and BOS.
Conclusions:
According to the results of this study, sintered bone substitute material remains histologically distinguishable but does not affect quantitative and qualitative bone regeneration.
More Related Videos
06:38Establishment of a Segmental Femoral Critical-size Defect Model in Mice Stabilized by Plate Osteosynthesis
Published on: October 12, 2016
09:34Visualizing Angiogenesis by Multiphoton Microscopy In Vivo in Genetically Modified 3D-PLGA/nHAp Scaffold for Calvarial Critical Bone Defect Repair
Published on: September 7, 2017