Base-triggered self-amplifying degradable polyurethanes with the ability to translate local stimulation to continuous
Yanhua Xu1, Samya Sen2, Qiong Wu1
1Department of Chemistry, University of Illinois at Urbana-Champaign Urbana Illinois 61801 USA sczimmer@illinois.edu.
Abstract:
A new type of base-triggered self-amplifying degradable polyurethane is reported that degrades under mild conditions, with the release of increasing amounts of amine product leading to self-amplified degradation. The polymer incorporates a base-sensitive Fmoc-derivative into every repeating unit to enable highly sensitive amine amplified degradation. A sigmoidal degradation curve for the linear polymer was observed consistent with a self-amplifying degradation mechanism. An analogous cross-linked polyurethane gel was prepared and also found to undergo amplified breakdown. In this case, a trace amount of localized base initiates the degradation, which in turn propagates through the material in an amplified manner. The results demonstrate the potential utility of these new generation polyurethanes in enhanced disposability and as stimuli responsive materials.
More Related Videos
15:33Microwave-assisted Functionalization of Polyethylene glycol and On-resin Peptides for Use in Chain Polymerizations and Hydrogel Formation
Published on: October 29, 2013
11:17Synthesis of Programmable Main-chain Liquid-crystalline Elastomers Using a Two-stage Thiol-acrylate Reaction
Published on: January 19, 2016
Related Concept Videos
Step-Growth Polymerization: Overview
Many natural and synthetic polymers are produced by...
Cationic Chain-Growth Polymerization: Mechanism
Anionic Chain-Growth Polymerization: Mechanism
Radical Chain-Growth Polymerization: Mechanism
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...