Related Experiment Video
Updated: Oct 30, 2025

Two-way Valorization of Blast Furnace Slag: Synthesis of Precipitated Calcium Carbonate and Zeolitic Heavy Metal Adsorbent
Published on: February 21, 2017
A Mathematical Model of the Expansion Evolution of Magnesium Oxide in Mass Concrete Based on Hydration
Chuqiao Feng1, Cheng Zhao2, Xiaomin Yu1
1Guizhou Engineering Technology Research Center for Exploitation and Utilization of Water Resources in Karst Region, Guiyang 550002, China.
Abstract:
The low swelling property of magnesium oxide concrete is a significant feature that can be used to control the cracking of mass concrete. Based on the characteristics of the chemical reaction, this work proposes a coupled hydro-thermo-mechanical model that can be implemented with the finite element method for predicting the autogenous volumetric deformation of magnesium concrete. By introducing the degree of the hydration reaction of magnesia and the degree of the hydration reaction of cementitious materials as intermediate variables of the chemical reaction system, a prediction model of the concrete temperature and chemical fields is established, and using this model, the effect of the temperature on the reaction rate can be considered in real time. In addition, by combining the relationship between the degree of the hydration reaction of magnesium oxide and the comprehensive expansion of concrete, a mathematical model for calculating the expansion stress of magnesia concrete was established. The algorithms were derived by mathematical equations, and the simulation results were compared to the experimental temperature and autogenous volumetric strain curves, which showed that the hydration model provides a relatively high accuracy. The model was also applied to an arch dam, and the coupled thermo-chemical-mechanical responses of mass concrete during construction were investigated. Simulation results show that the increase in temperature (hydration of cementitious material) and expansion volumetric deformation (hydration of MgO) of the concrete on the upstream and downstream surfaces lags obviously behind that of the inner regions. Quantitative analysis for differences of internal and external expansion is worthy of further attention and study on a basis of further experimental data as well as monitored data.
Related Concept Videos
Dynamic Modulus of Elasticity of Concrete
The sonic test is a common method to determine the dynamic modulus. In this test, a concrete beam, sized either 6 x 6 x 30 inches or 4 x 4 x 20 inches, is clamped at its center. Vibrations are initiated at one end of the beam by an electromagnetic exciter unit powered by...
Hydration of Cement
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
Alkali Aggregate Reaction in Concrete
Soundness of Cement
Carbonation Shrinkage
The concrete's permeability is slightly reduced as calcium carbonate produced during the reaction fills its pores. Furthermore, its strength is slightly enhanced as the water released during the reaction...