Impact of Fabrication Techniques and Polishing Procedures on Surface Roughness of Denture Base Resins
Published on: January 17, 2025
Comparison of the Masticatory Force (with 3D Models) of Complete Denture Base Acrylic Resins with Reline and
Catarina Calamote1, Isabel Carolina Coelho1, António Sérgio Silva2
1Department of Oral Rehabilitation, Instituto Universitário de Ciências da Saúde, 4585-116 Gandra, Portugal.
Abstract:
The reinforcement of acrylic denture base remains problematic. Acrylic prosthesis fractures are commonly observed in prosthodontic practice and have not been reliably resolved. This study compared the resistance to masticatory force of acrylic bases of removable complete conventional prosthesis in 3D upper models. Forty acrylic base test specimens containing two types of reinforcement meshes (20 with glass fiber meshes (FIBER-FORCE®- Synca, Bio Composants MédicauxTM, Tullins, France), 20 with metal meshes (DENTAURUM®-Ispringen, Germany)), 20 with a conventional PMMA acrylic base (LUCITONE 199®-Dentsply Sirona, York, PA, USA), and 20 using a permanent soft reline material (MOLLOPLAST-B®-DETAX GmbH & Co. KG, Ettlingen, Germany) were tested-a total of 80 specimens. Half of the specimens were made for a low alveolar ridge and half for a high alveolar ridge. The data were analysed using one-way analysis of variance and Student's t-test for independent test specimens. In the high-alveolar-ridge group, the prosthesis reinforced with the glass fiber mesh was the most resistant to fracture, while in the low-alveolar-ridge group, the non-reinforced prosthesis showed the highest resistance masticatory force. Prostheses with the permanent soft reline material showed the lowest resistance to fracture in both high and low-alveolar-ridge groups. The results show that the selection of the right reinforcement material for each clinical case, based on the height of the alveolar ridge, may help to prevent prosthesis fractures.