Concrete Modular Pavement Structures with Optimized Thickness Based on Characteristics of High Performance Concrete
Audrius Vaitkus1, Judita Gražulytė1, Ovidijus Šernas1
1Road Research Institute, Vilnius Gediminas Technical University, 08217 Vilnius, Lithuania.
Abstract:
Usually, C30/37 strength class concrete is used to construct concrete pavements on a rigid, semi-rigid or flexible base. Concrete with such a strength delivers essential design characteristics: flexural strength and tensile splitting strength are between 4.5-5.4 MPa and 2.8-3.7 MPa, respectively. Design characteristics can be significantly increased by densifying the concrete mixture, i.e., adding silica fume, steel or polypropylene macro fibers. As high-performance concrete characteristics are 20-60% higher than those for standard concrete (C30/37), new possibilities to reduce the thickness of concrete pavement slabs appear. The theoretical analysis of concrete pavement structures with high-performance concrete mixtures (C40/50, C45/55 and C50/60) showed that slab thickness could be reduced by 6-39% compared to a standard concrete pavement structure depending on the concrete properties and design method. From all those pavement structures, three concrete mixtures were determined as the most rational ones in terms of PCP thickness reduction and total pavement cost: (i) with 49.5 kg/m3 of steel fibers and 25.2 kg/m3 of silica fume; (ii) with 10.0 kg/m3 of polypropylene fibers (type A); (iii) with 49.5 kg/m3 of steel fibers.
More Related Videos
Related Concept Videos
Fiber Reinforced Concrete
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen...
Additives and Fillers in Concrete
The...
Design Example: Joints in Concrete Pavements
Contraction joints are typically formed by sawing a groove into the concrete shortly after it has hardened. This creates a weakened vertical plane, deliberately encouraging cracking at...
Fatigue Strength of Concrete
Frost Resistant Concrete
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...