Abstract:
This paper mainly demonstrates an advanced type of the vaporizing foil actuator welding (VFAW) process between GPa-grade steel (TRIP1180) and aluminum alloy (AA5052-H32) without applying standoff. To secure a flying distance during the VFAW process, the preformed target sheet shaped like a circular indentation has been utilized. It is necessary to optimize process parameters integrated with geometrical design of the preform since the welding strength can be decreased beyond the optimum input energy in the standoff-free VFAW process. The welded surface was evaluated by SEM-EDS, XRD, EBDS, and TEM to analyze the welding mechanism and composition at the welding interface. The diffusion zone including the AlFe3 phase was observed at the welded interface which has high grain density due to the high-speed impact by increasing the welding strength, which leads to the perfect welding between the dissimilar materials.
More Related Videos
08:40Ultrasonic Welding of Thermoplastic Composite Coupons for Mechanical Characterization of Welded Joints through Single Lap Shear Testing
Published on: February 11, 2016
10:52Conducting Elevated Temperature Normal and Combined Pressure-Shear Plate Impact Experiments Via a Breech-end Sabot Heater System
Published on: August 7, 2018