Prevention of Hematite Settling in Water-Based Mud at High Pressure and High Temperature

Ashraf Ahmed1, Salem Basfar1, Theis I Solling1

  • 1College of Petroleum Engineering and Geosciences, King Fahd University of Petroleum & Minerals, Dhahran 31261, Saudi Arabia.

ACS Omega
|September 22, 2021
PubMed

Related Concept Videos

Coagulation01:06

Coagulation

Colloidal solids are solid particles suspended in solution. They are usually negatively charged, attracting a compact primary layer of positively charged ions, which attract more counterions to form an electrical double layer. Electrostatic repulsion between the charged double layers prevents the particles from colliding, stabilizing the colloids. These solids are often undesirable because they can contain toxins that are difficult to remove. Coagulation is a technique that helps aggregate and...
482
Colloidal precipitates01:09

Colloidal precipitates

The high insolubility of some precipitates can result in an unfavorable relative supersaturation. This can lead to colloidal particles with a large surface-to-mass ratio, where adsorption is promoted. For instance, in the precipitation of silver chloride, silver ions are adsorbed on the surface of the colloidal particles, forming a primary layer. This layer attracts ions of opposite charge (such as nitrate ions), forming a diffuse secondary layer of adsorbed ions. This electric double layer...
1.1K
Precipitation and Co-precipitation01:17

Precipitation and Co-precipitation

Precipitation and coprecipitation methods can be used to separate a mixture of ions in a solution. In qualitative inorganic analysis, ions that form sparingly soluble precipitates with the same reagent are separated based on the differences in solubility products. For example, consider the separation of Cu(II) and Fe(II) ions by precipitation as insoluble sulfides. First, copper(II) sulfide is precipitated by the addition of acidic H2S, where the dissociation of H2S is suppressed. Adding H2S...
2.8K
Hot Weather Concreting01:20

Hot Weather Concreting

Concreting at elevated temperatures accelerates the hydration process, leading to quicker setting but potentially reducing the long-term strength of the concrete structure. Additionally, low air humidity fosters rapid moisture loss from the concrete, resulting in reduced workability, pronounced plastic shrinkage, and a higher likelihood of crazing.
Mitigating the heat increase in concrete can be economically achieved by shading aggregate stockpiles to prevent heating from solar radiation,...
143
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
212
Washing, Drying, and Ignition of Precipitates00:52

Washing, Drying, and Ignition of Precipitates

After filtration, the precipitate is washed to remove coprecipitated impurities and any remaining mother liquor. Colloidal precipitates, such as silver chloride, are washed with an electrolyte (such as dilute nitric acid) to prevent the peptization of the precipitate. In the case of slightly soluble precipitates, the wash solution contains a common ion to reduce solubility. Lead sulfate, which is slightly soluble in water, is washed with dilute sulfuric acid. Similarly, wash solutions may be...
1.5K