Surface analysis of novel fibroin films based on well-preserved crystalline structures
Yoko Okahisa1, Chieko Narita1, Takashi Aoki1
1Faculty of Fiber Science and Engineering, Kyoto Institute of Technology, Matsugasaki, Sakyo, Kyoto 606-8585, Japan.
Abstract:
We recently reported that a highly homogeneous aqueous suspension of fibroin nanofiber (FNF) can be simply obtained by mechanical water-grinding a heterogeneous aqueous fibroin slurry and that the FNF in the suspension preserves the native β-sheet secondary structure during this mechanical treatment. The current study reports the surface properties of well-preserved crystalline structure novel FNF film from water-grinding preparation as compared with those of typical, conventionally prepared regenerated fibroin (RF) film. RF film was not treated with alcoholic solutions and was verified to be amorphous from a WAXD diffraction diagram. The air-side surfaces of the FNF semi-crystalline and RF amorphous films were studied to clarify differences using scanning electron microscopy (SEM), atomic force microscopy (AFM), attenuated total reflection Fourier transform infrared spectroscopy (ATR-FTIR), static water contact angle, and X-ray photoelectron spectroscopy (XPS). The well-preserved crystalline in the FNF film was found to exist near a slightly deep surface region and to act as a physically cross-linking domain, governing the molecular motions of the amorphous polypeptide chains at the very shallow surface region.
Related Concept Videos
Fibrous Proteins
Globular and Fibrous Proteins
Globular proteins are also known as spheroproteins and typically are approximately round in shape. They contain a mix of amino acid types and contain differing sequences in their primary structures. Globular proteins have many different functions, such as enzymes, cellular messengers, and molecular transporters. These roles often require the proteins to be...