Purpose:
The aim of this study was to evaluate flexural strength, elastic modulus and dynamic mechanical analysis (DMA) of heat-polymerized polymethyl methacrylate resin, polyamide resin and glass fiber-reinforced polyamide resin.
Materials And Methods:
Three groups were determined according to denture base materials as polymethyl methacrylate resin (H), polyamide resin (P) and glass fiber reinforced polyamide resin (R). Sixteen specimens for each denture base material were prepared with dimensions of 64x10x3.3 mm for three-point bending test. Two specimens for each denture base material were prepared with dimensions of 30x10x3 mm for DMA. Polymethyl methacrylate and polyamide specimens were prepared according to the manufacturer's recommendations. The silane was applied to glass fibers (4.5 mm length) 2% by weight of the polyamide resin, they were placed in polyamide resin cartilages and injected to the mold. The thermal aging procedure was applied to half of specimens of each material (n=8). Flexural strength and elastic modulus of the specimens were determined by three-point bending test at a speed of 5 mm/ min. DMA was performed to 1 specimen from each group to evaluate viscoelastic properties. Data were analyzed with one-way ANOVA, Tukey and Paired t tests.
Results:
A statistically significant difference was found in flexural strength and elastic modulus values of denture base materials (p=0.00). The highest flexural strength and elastic modulus values were observed in polymethyl methacrylate group. There was no significant difference between polyamide and glass-fiber reinforced polyamide groups (p=0.497). No significant difference was determined in all threedenture base materials before and after aging procedure.
Conclusion:
The reinforcement with glass-fibers did not affect the flexural strength and elastic modulus of polyamide resin.
Related Concept Videos
Fiber Reinforced Concrete
Flexural Stress
Hooke's Law states that within the material's elastic limits, stress is directly proportional to strain. In a member experiencing a bending moment, the strain at any point is relative to...
Members Made of Elastoplastic Material
As the bending moment...
Bending of Members Made of Several Materials
Hooke's Law determines stress in each material, stating that stress is proportional to strain but varies due to each...
Dynamic Modulus of Elasticity of Concrete
The sonic test is a common method to determine the dynamic modulus. In this test, a concrete beam, sized either 6 x 6 x 30 inches or 4 x 4 x 20 inches, is clamped at its center. Vibrations are initiated at one end of the beam by an electromagnetic exciter unit powered by...
Residual Stresses in Bending