Data on the occurrence of a Brass texture and elastic anisotropy in laser blown powder processed superalloy IN718
J F S Markanday1, M A Carpenter2, R P Thompson1
1Department of Materials Science & Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge CB3 0FS, UK.
Abstract:
The additive manufacturing (AM) of components through laser-blown-powder directed-energy-deposition (LBP-DED) is highly applicable to the repair of aerospace components. Fabrication of superalloys with this technique, as with other AM methods, often encounters complications that include the formation of undesired phases, irregular microstructure and texture leading to anisotropic elastic properties. Heat treatments and other post-processing techniques can be used to mitigate these issues. The collected data demonstrates the effects of different heat treatment protocols on the microstructure, elastic properties, and hardness of LBP-DED IN718. In this study eight different heat treatment were used to investigate the effects of treatment time and temperature. The microstructure was investigated through SEM, with XRD and EDX used for phase analysis. The texture was characterised using SEM coupled with EBSD and the elastic properties were determined from resonant ultrasound spectroscopy.
Related Concept Videos
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Plastic Behavior
Yield Criteria for Ductile Materials under Plane Stress
The Maximum Shearing Stress Criterion, also known as...
Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity
Temperature Dependent Deformation
Hooke's Law