Related Experiment Video
Updated: Oct 4, 2025

Growth and Electrostatic/chemical Properties of Metal/LaAlO3/SrTiO3 Heterostructures
Published on: February 8, 2018
Ambient pressure x-ray photoelectron spectroscopy setup for synchrotron-based in situ and operando atomic layer
E Kokkonen1, M Kaipio2, H-E Nieminen2
1MAX IV Laboratory, Lund University, Box 118, 221 00 Lund, Sweden.
Abstract:
An ambient pressure cell is described for conducting synchrotron-based x-ray photoelectron spectroscopy (XPS) measurements during atomic layer deposition (ALD) processes. The instrument is capable of true in situ and operando experiments in which it is possible to directly obtain elemental and chemical information from the sample surface using XPS as the deposition process is ongoing. The setup is based on the ambient pressure XPS technique, in which sample environments with high pressure (several mbar) can be created without compromising the ultrahigh vacuum requirements needed for the operation of the spectrometer and the synchrotron beamline. The setup is intended for chemical characterization of the surface intermediates during the initial stages of the deposition processes. The SPECIES beamline and the ALD cell provide a unique experimental platform for obtaining new information on the surface chemistry during ALD half-cycles at high temporal resolution. Such information is valuable for understanding the ALD reaction mechanisms and crucial in further developing and improving ALD processes. We demonstrate the capabilities of the setup by studying the deposition of TiO2 on a SiO2 surface by using titanium(IV) tetraisopropoxide and water as precursors. Multiple core levels and the valence band of the substrate surface were followed during the film deposition using ambient pressure XPS.
More Related Videos
09:00Experimental Methods for Spin- and Angle-Resolved Photoemission Spectroscopy Combined with Polarization-Variable Laser
Published on: June 28, 2018
10:03Characterization of Electrode Materials for Lithium Ion and Sodium Ion Batteries Using Synchrotron Radiation Techniques
Published on: November 11, 2013
Related Concept Videos
Atomic Emission Spectroscopy: Instrumentation
Atomic Emission Spectroscopy: Lab
Inductively Coupled Plasma Atomic Emission Spectroscopy: Instrumentation
There are three main types of inductively coupled plasma atomic emission spectroscopy (ICP-AES) instruments: sequential, simultaneous multichannel, and Fourier transform instruments, with the latter being less commonly used....
Atomic Absorption Spectroscopy: Atomization Methods
Atomic Absorption Spectroscopy: Radiation and Light Sources
Two common narrow-range 'line' sources used in AAS are hollow-cathode lamps (HCLs) and...
Atomic Absorption Spectroscopy: Instrumentation
The atomizer used in AAS can be either a flame atomizer or an...