Efficient compressed database of equilibrated configurations of ring-linear polymer blends for MD simulations

Katsumi Hagita1, Takahiro Murashima2, Masao Ogino3

  • 1Department of Applied Physics, National Defense Academy, 1-10-20, Hashirimizu, Yokosuka, 239-8686, Japan. hagita@nda.ac.jp.

Scientific Data
|February 9, 2022
PubMed

Related Concept Videos

Polymers: Molecular Weight Distribution01:10

Polymers: Molecular Weight Distribution

For any given polymer, the weight average molecular weight (Mw) is higher than, if not equal to, the number average molecular weight (Mn). The only situation in which the weight average molecular weight and the number average molecular weight are equal is when a polymer consists only of chains with equal molecular weight. However, this never happens in a synthetic polymer, since it is difficult to control the polymerization process up to a molecular level with accuracy to a hundred percent.
4.0K
Molecular Weight of Step-Growth Polymers01:08

Molecular Weight of Step-Growth Polymers

Step growth polymerization involves bi or multifunctional monomers. Bifunctional monomers react to form linear step growth polymers, whereas multifunctional monomers react to form non-linear or branched polymers.
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
2.4K
¹H NMR of Conformationally Flexible Molecules: Temporal Resolution00:52

¹H NMR of Conformationally Flexible Molecules: Temporal Resolution

At room temperature, the chair conformer of cyclohexane undergoes rapid ring flipping between two equivalent chair conformers at a rate of approximately 105 times per second. These two chair conformers are in equilibrium. The rapid ring flipping results in the interconversion of the axial proton to an equatorial proton and an equatorial to the axial proton. Such interconversions are too rapid and cannot be detected on the NMR timescale. Hence, the NMR spectrometer cannot distinguish between the...
946
Polymers: Defining Molecular Weight01:01

Polymers: Defining Molecular Weight

Unlike small molecules with definite molecular weights, polymers are a mixture of individual polymer chains of varying lengths, each with a unique molecular weight.  So, the molecular weight of a polymer is expressed as an average value based on the average size of the polymer chains. The two most common forms of averages used for polymers are the number average molecular weight and weight average molecular weight.
The number average molecular weight (Mn) is the summation of the number...
3.3K
Polymer Classification: Crystallinity01:21

Polymer Classification: Crystallinity

Unlike ionic or small covalent molecules, polymers do not form crystalline solids due to the diffusion limitations of their long-chain structures. However, polymers contain microscopic crystalline domains separated by amorphous domains.
Crystalline domains are the regions where polymer chains are aligned in an orderly manner and held together in proximity by intermolecular forces. For example, chains in the crystalline domains of polyethylene and nylon are bound together by van der Waals...
3.2K
¹H NMR of Conformationally Flexible Molecules: Variable-Temperature NMR01:15

¹H NMR of Conformationally Flexible Molecules: Variable-Temperature NMR

The axial and equatorial protons in cyclohexane can be distinguished by performing a variable-temperature NMR experiment. In this process, except for one proton, the remaining eleven protons are replaced by deuterium. The deuterium substitution avoids the possible peak splitting caused by the spin-spin coupling between the adjacent protons. The remaining proton flips between the axial and equatorial positions.
1.2K