Experimental Study on Strength Enhancement of Expansive Grout
Di Wang1, Yicheng Ye1,2, Nan Yao1,2
1School of Resources and Environmental Engineering, Wuhan University of Science and Technology, Wuhan 430081, China.
Abstract:
Adding an expansive agent to ordinary grout can cause an expansion in volume, but also reduces its strength. In order to improve the strength of expansive grout, quartz sand is used as the strength enhancement additive. In this study, the expansion behavior and mechanical properties of the expansive grout with quartz sand are explored, through expansion development monitoring, uniaxial compression strength (UCS), acoustic emission (AE), SEM and XRD test methods. The results showed that: (1) The final expansion ratio and expansion development of the samples are related to the use of an expansive agent, but not affected by quartz sand. With the increase in expansion agent content, the average expansion ratios of the samples are 0.03%, 0.16%, 0.67%, 1.06% and 1.48%; (2) The UCS of the samples decreases with the increase in expansive agent content but increases with the increase in quartz sand content. Compared with no quartz sand, and with the increase in quartz sand content, the average strength of the samples increased by 10.51%, 29.88%, and 37.92%; (3) Quartz sand does not effectively participate in the hydration reaction, but it can effectively enhance the strength of the expansive grout without affecting its volume expansion, which makes it an ideal expansive grout strength enhancement additive.
More Related Videos
Related Concept Videos
Bonding and Strength of Aggregate
Reinforced Brick Masonry
To fortify brick walls...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Impact Strength of Concrete
Superplasticizers
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen...