Highly stable Pt-Co bimetallic catalysts prepared by atomic layer deposition for selective hydrogenation of

Kaiying Wang1, Xiaoqing He2,3, Jee-Ching Wang1

  • 1Linda and Bipin Doshi Department of Chemical and Biochemical Engineering, Missouri University of Science and Technology, Rolla, MO 65409, United States of America.

Nanotechnology
|February 15, 2022
PubMed

Related Concept Videos

Reduction of Alkenes: Asymmetric Catalytic Hydrogenation02:17

Reduction of Alkenes: Asymmetric Catalytic Hydrogenation

Catalytic hydrogenation of alkenes is a transition-metal catalyzed reduction of the double bond using molecular hydrogen to give alkanes. The mode of hydrogen addition follows syn stereochemistry.
The metal catalyst used can be either heterogeneous or homogeneous. When hydrogenation of an alkene generates a chiral center, a pair of enantiomeric products is expected to form. However, an enantiomeric excess of one of the products can be facilitated using an enantioselective reaction or an...
3.5K
Reduction of Alkenes: Catalytic Hydrogenation02:13

Reduction of Alkenes: Catalytic Hydrogenation

Alkenes undergo reduction by the addition of molecular hydrogen to give alkanes. Because the process generally occurs in the presence of a transition-metal catalyst, the reaction is called catalytic hydrogenation.
Metals like palladium, platinum, and nickel are commonly used in their solid forms — fine powder on an inert surface. As these catalysts remain insoluble in the reaction mixture, they are referred to as heterogeneous catalysts.
The hydrogenation process takes place on the...
12.7K
Reduction of Alkynes to cis-Alkenes: Catalytic Hydrogenation02:24

Reduction of Alkynes to cis-Alkenes: Catalytic Hydrogenation

Introduction
Like alkenes, alkynes can be reduced to alkanes in the presence of transition metal catalysts such as Pt, Pd, or Ni. The reaction involves two sequential syn additions of hydrogen via a cis-alkene intermediate.
8.2K
Reduction of Benzene to Cyclohexane: Catalytic Hydrogenation01:28

Reduction of Benzene to Cyclohexane: Catalytic Hydrogenation

Unlike the easy catalytic hydrogenation of an alkene double bond, hydrogenation of a benzene double bond under similar reaction conditions does not take place easily. For example, in the reduction of stilbene, the benzene ring remains unaffected while the alkene bond gets reduced. Hydrogenation of an alkene double bond is exothermic and a favorable process. In contrast, to hydrogenate the first unsaturated bond of benzene, an energy input is needed; that is, the process is endothermic. This is...
5.1K
Radical Substitution: Hydrogenolysis of Alkyl Halides with Tributyltin Hydride01:26

Radical Substitution: Hydrogenolysis of Alkyl Halides with Tributyltin Hydride

Radical substitution reactions can be used to remove functional groups from molecules. The hydrogenolysis of alkyl halides is one such reaction, where the weak Sn–H bond in tributyltin hydride reacts with alkyl halides to form alkanes. Here, the reagent Bu3SnH yields tributyltin halide as a byproduct.
The bonds formed in this reaction are stronger than the bonds broken, making it energetically favorable. The reaction follows a radical chain mechanism similar to radical halogenation...
1.9K
Alcohols from Carbonyl Compounds: Reduction02:23

Alcohols from Carbonyl Compounds: Reduction

Reduction is a simple strategy to convert a carbonyl group to a hydroxyl group. The three major pathways to reduce carbonyls to alcohols are catalytic hydrogenation, hydride reduction, and borane reduction.
Catalytic hydrogenation is similar to the reduction of an alkene or alkyne by adding H2 across the pi bond in the presence of transition metal catalysts like Raney Ni, Pd–C, Pt, or Ru. Aldehydes and ketones can be reduced by this method, often under mild to moderate heat (25–100°C) and...
11.0K