Related Experiment Video
Updated: Oct 1, 2025

Harvesting Solar Energy by Means of Charge-Separating Nanocrystals and Their Solids
Published on: August 23, 2012
Activating a Semiconductor-Liquid Junction via Laser-Derived Dual Interfacial Layers for Boosted Photoelectrochemical
Jie Jian1,2, Shiyuan Wang1,2, Qian Ye1,2
1State Key Laboratory of Solidification Processing, Center for Nano Energy Materials, School of Materials Science and Engineering, Analytical and Testing Center, Northwestern Polytechnical University and Shaanxi Joint Laboratory of Graphene (NPU), Xi'an, 710072, P. R. China.
Abstract:
The semiconductor-liquid junction (SCLJ), the dominant place in photoelectrochemical (PEC) catalysis, determines the interfacial activity and stability of photoelectrodes, whcih directly affects the viability of PEC hydrogen generation. Though efforts dedicated in past decades, a challenge remains regarding creating a synchronously active and stable SCLJ, owing to the technical hurdles of simultaneously overlaying the two advantages. The present work demonstrates that creating an SCLJ with a unique configuration of the dual interfacial layers can yield BiVO4 photoanodes with synchronously boosted photoelectrochemical activity and operational stability, with values located at the top in the records of such photoelectrodes. The bespoke dual interfacial layers, accessed via grafting laser-generated carbon dots with phenolic hydroxyl groups (LGCDs-PHGs), are experimentally verified effective, not only in generating the uniform layer of LGCDs with covalent anchoring for inhibited photocorrosion, but also in activating, respectively, the charge separation and transfer in each layer for boosted charge-carrier kinetics, resulting in FeNiOOH-LGCDs-PHGs-MBVO photoanodes with a dual configuration with the photocurrent density of 6.08 mA cm-2 @ 1.23 VRHE , and operational stability up to 120 h @ 1.23 VRHE . Further work exploring LGCDs-PHGs from catecholic molecules warrants the proposed strategy as being a universal alternative for addressing the interfacial charge-carrier kinetics and operational stability of semiconductor photoelectrodes.
More Related Videos
08:48Selective Area Modification of Silicon Surface Wettability by Pulsed UV Laser Irradiation in Liquid Environment
Published on: November 9, 2015
11:26Integrating a Triplet-triplet Annihilation Up-conversion System to Enhance Dye-sensitized Solar Cell Response to Sub-bandgap Light
Published on: September 12, 2014
Related Concept Videos
Metal-Semiconductor Junctions
Schottky Barriers
Schottky barriers arise when a metal with a work function (Φm) contacts a semiconductor with a different work function (Φs). Initially, electrons transfer until the Fermi levels of the metal and semiconductor align at equilibrium. For instance, if Φm > Φs, the semiconductor Fermi level is higher than the metal's before contact. The...
P-N junction
Biasing of Metal-Semiconductor Junctions
In Schottky junctions, where the semiconductor is n-type, applying a positive voltage to the metal relative to the semiconductor reduces its Fermi...