Catalytic effect of diesel PM derived ash on PM oxidation activity
Jianbing Gao1, Yufeng Wang2, Xiaopan Li3
1School of Mechanical Engineering, Beijing Institute of Technology, Beijing, 10081, China; Key Laboratory of Shaanxi Province for Development and Application of New Transportation Energy, Xi'an, 710064, China.
Abstract:
With diesel particulate filter and gasoline particulate filter periodical regeneration, more and more ash accumulates on the substrate of filter. Ash gathering on the substrate of filter leads to more contact area of particulate matter and ash. Specific ingredients in ash present catalytic effects on particulate matter oxidation. However, the catalytic effect of diesel particulate matter derived ash on its oxidation, mimicking the ash accumulating on filter substrate, is still uncovered using experiments. In this paper, diesel particulate matter derived ash was put at the bottom of particulate matter samples to imitating the soot loading on filter substrate which was covered by much ash. The results indicated that the burnout temperature of diesel particulate matter was in the range of 500-600 °C; while it was 600-700 °C for Printex (U). The burnout temperature drop by ash was lower than 10 °C for diesel particulate matter. The maximum mass loss rate corresponded to approximately 450 °C for diesel particulate matter, and it was changed minorly by ash and ramp rates. However, the temperature corresponding to the maximum mass loss rate was seriously retarded by high ramp rates for Printex (U), and ash presented limited effect on it. The maximum activation energy drop by ash was approximately 60 kJ/mol at the initial stage of oxidation for diesel particulate matter. The activation energy was approximately 132.19, 114.78, 157.26, and 144.67 kJ/mol for diesel PM, diesel PM-ash, Printex (U), and Printex (U)-ash, respectively. Organic compounds dropped gradually in the oxidation process of diesel particulate matter. Nanostructure evolutions of diesel particulate matter and Printex (U) were similar, experiencing smaller sizes and void cores at the end of oxidation process.
Related Concept Videos
Catalysis
Oxidation of Alkenes: Anti Dihydroxylation with Peroxy Acids
Oxidation of Alkenes: Syn Dihydroxylation with Potassium Permanganate
Oxidation of Alkenes: Syn Dihydroxylation with Osmium Tetraoxide
Oxidations of Aldehydes and Ketones to Carboxylic Acids
Aldehydes readily undergo oxidation in strong oxidizing agents such as potassium permanganate and chromic acid. The oxidation can also be carried out using mild oxidizing agents such as silver oxide. In fact, aldehydes can be easily oxidized...
Radical Autoxidation