Related Experiment Video
Updated: Sep 27, 2025

Advanced Compositional Analysis of Nanoparticle-polymer Composites Using Direct Fluorescence Imaging
Published on: July 19, 2016
Three-Dimensional Nanoscale Morphological Surface Analysis of Polymeric Particles Containing Allium sativum Essential
Larissa Medeiros de Oliveira1, Robert Saraiva Matos2,3, Ştefan Ţălu4
1Laboratory of Nanostructured Polymers (NANOPOL-@nanopol_ufam), Department of Physics, Federal University of Amazonas (UFAM), Manaus 69067-005, AM, Brazil.
Abstract:
Biodegradable particles were developed using poly-ε-caprolactone and gelatin carriers containing different concentrations of Allium sativum essential oil (EO) (360 µg/mL, 420 µg/mL, and 460 µg/mL). Atomic force microscopy was useful to evaluate the particles' surface based on morphological parameters. The particles' size varied from 150 nm to 300 nm. The diameter was related to the increase of the particles' height as a function of the EO concentration, influencing the roughness of the surface core values (from 20 to 30 nm) and surface irregularity. The spatial parameters Str (texture aspect ratio) and Std (texture direction) revealed low spatial frequency components. The hybrid parameters Sdq (root mean square gradient) and Sdr (interfacial area ratio) also increased as a function of the EO concentration, revealing fewer flat particles. On the other hand, the functional parameters (inverse areal material ratio and peak extreme height) suggested differences in surface irregularities. Higher concentrations of EO resulted in greater microtexture asperity on the particles' surface, as well as sharper peaks. The nanoscale morphological surface analysis allowed the determination of the most appropriate concentration of encapsulated EO, influencing statistical surface parameters.
More Related Videos
06:54Author Spotlight: Advances in Nanoscale Infrared Spectroscopy to Explore Multiphase Polymeric Systems
Published on: June 23, 2023
10:10Three-Dimensional Particle Shape Analysis Using X-ray Computed Tomography: Experimental Procedure and Analysis Algorithms for Metal Powders
Published on: December 4, 2020