Practical method to determine the effective zero-point of indentation depth for continuous stiffness measurement

Diancheng Geng1,2, Hao Yu1, Yasuki Okuno1

  • 1Institute for Materials Research, Tohoku University, Sendai, Miyagi, 980-8577, Japan.

Scientific Reports
|April 17, 2022