Abrasive Wear of Mining Chain Drums Made of Austempered Ductile Iron in Different Operating Modes
Andrzej N Wieczorek1, Mateusz Wójcicki2, Andrzej Drwięga2
1Faculty of Mining, Safety Engineering and Industrial Automation, Silesian University of Technology, Akademicka 2 Street, 44-100 Gliwice, Poland.
Abstract:
The paper presents results of testing the resistance of chain wheels made of alloyed austempered ductile iron (ADI) with various content of retained austenite and subjected to shot peening, to the dynamic and abrasive wear by solid particles. The impact of the additional environmental factor-external dynamic forces-accompanying the operation of the chain wheels in the presence of the quartz particles has a synergistic effect on the abrasive wear in the contact area between the wheels and the chain links for all the considered variants, except for the ADI with the structure of the upper ausferrite. Based on the results obtained, it was found that the abrasive wear by solid particles increased and that the hardness of the surface layer of the chain wheels subjected to shot peening decreased. The relative increase in the wear ΔVDYN/δMAX,(A), representing the share of the additional dynamic force in the process of wear, was in the range of 16-40% for the group of tested cast iron ADI not subjected to shot peening, while for the shot peened-in the range of 16-64%. Demonstration of phase changes during the operation of chain wheels and the change in their intensity depending on the combination of environmental factors is the work novelty. In the opinion of the authors, the presented results will be of great practical importance as they will allow to increase the knowledge on the proper selection of ADI cast iron for environmental conditions.
More Related Videos
07:47Experimental Protocol to Investigate Particle Aerosolization of a Product Under Abrasion and Under Environmental Weathering
Published on: September 16, 2016
08:58Atomic Force Microscopy Cantilever-Based Nanoindentation: Mechanical Property Measurements at the Nanoscale in Air and Fluid
Published on: December 2, 2022
Related Concept Videos
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Quarrying of Stone
One common method involves using a diamond belt saw to cut large blocks from the quarry face. These blocks can be about 50 feet long and 12 feet high. After the initial vertical cut, drilling is performed at the base of the...
Fatigue
Toughness and Hardness of Aggregate
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Characteristics of Dry Friction
Before the wheelbarrow starts moving, the static frictional force acts tangentially to the contact surface, opposing the force that is about to induce the motion. This frictional force prevents the...