Portevin-Le Châtelier Effect in a Powder Metallurgy Co-Ni-Based Superalloy
Chao Li1, Jianwei Teng1, Biaobiao Yang1,2,3
1State Key Laboratory for Powder Metallurgy, Central South University, Changsha 410083, China.
Abstract:
The Portevin-Le Châtelier (PLC) effect in a powder metallurgy (PM) Co-Ni-based superalloy was systematically investigated via the tensile tests at temperatures ranging from 200 to 600 °C and strain rates at 1.0 × 10-4 to 1.0 × 10-2. Both normal and inverse PLC effects were observed in the PLC regime, and the former appeared in the A and B types at a low temperature, whilst the latter appeared in the C type at an elevated temperature. Both positive and negative strain rate sensitivities (SRS) were shown in PLC regime, and SRS should be derived from same types of serrations. Based on the calculated activation energy, the substitutional atom Mo is considered to take primary responsibility for the PLC effect in present alloy.
Related Concept Videos
Le Chatelier's Principle: Changing Temperature
To understand this phenomenon, consider the elementary reaction:
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Le Chatelier's Principle: Changing Volume (Pressure)