Study on Deterioration Law and Mechanism of Gray Brick Due to Salt Crystallization

Jianwei Yue1,2,3, Yuan Li1, Zhenxian Luo1,2

  • 1School of Civil Engineering and Architecture, Henan University, Kaifeng 475004, China.

Related Concept Videos

Mortar Joint Deterioration in Masonry01:13

Mortar Joint Deterioration in Masonry

Mortar joint deterioration is a significant concern in masonry structures, with water accumulation in the joints leading to damage from freeze-thaw cycles. The repeated expansion of water during freezing and its melting during thawing develop and propagate cracks in the masonry joints. Eventually, this leads to the spalling of mortar from the joints, loosening masonry units and weakening the structure. The deteriorated mortar joints are also vulnerable to moisture intrusion into the walls.
The...
169
Brick Durability, Strength, and Appearance01:15

Brick Durability, Strength, and Appearance

Brick durability, strength, and appearance are crucial factors in construction, influencing the choice of bricks for specific applications. The process of freeze-thaw, for instance, significantly affects brick durability. This phenomenon occurs when water absorbed by a brick expands as it freezes, potentially causing damage when it melts and refreezes. Bricks are graded for durability: SW-grade bricks are the most durable, offering high strength and low water absorption, followed by MW-grade...
411
Effect of Sea Water on Concrete01:22

Effect of Sea Water on Concrete

Concrete exposed to seawater can undergo degradation like the dissolution of ettringite and gypsum, increasing the material's porosity and decreasing its strength. In contrast, the crystallization of salts within the concrete's pores can cause expansion, particularly above the waterline where evaporation occurs. Nonetheless, this expansion only happens when seawater, enabled by the concrete's permeability, manages to infiltrate the structure.
Concrete in areas between tide marks,...
504
Efflorescence in Masonry01:25

Efflorescence in Masonry

Efflorescence in masonry walls appears as a fluffy crystalline powder, often white, resulting from water-soluble salts within the masonry or mortar. When water penetrates the masonry, it dissolves these salts and brings them to the surface, where they are deposited upon evaporation of water.
While initial efflorescence is common post-construction and can be cleaned with water and a brush, in certain instances, efflorescence can reappear and gradually diminish over time as salts are leached out...
156
Deleterious Substances in Aggregate01:25

Deleterious Substances in Aggregate

Deleterious substances in aggregates can be detrimental to the quality and durability of concrete. These substances include organic impurities like loam, which interfere with cement hydration and are usually present in the sand. These prevent a good bond between aggregate and cement paste. Organic impurities can be detected using the colorimetric test, where the darkness of a solution after agitation indicates the level of organic content.
Another type of impurity is clay and fine material that...
275
Unsoundness of Aggregate due to Volume Change01:26

Unsoundness of Aggregate due to Volume Change

Unsoundness in aggregates due to volume changes is primarily caused by the physical alterations aggregates undergo, such as freezing and thawing, thermal changes, and wetting and drying. Unsound aggregates, when subjected to these changes, result in volume change upon disintegration. This, in turn, contributes to the deterioration of concrete, including scaling, pop-outs, and cracking. Particular types of aggregates, such as porous flints, cherts, and those containing clay minerals, are...