Corrosion behavior of 904L austenitic stainless steel in hydrofluoric acid

Guobo Zou1, Wei Shi1, Song Xiang1,2

  • 1College of Materials and Metallurgy, Guizhou University Guiyang 550025 China sxiang@gzu.edu.cn.

RSC Advances
|May 11, 2022
PubMed

Related Concept Videos

Corrosion of Reinforcement01:27

Corrosion of Reinforcement

The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
264
Corrosion02:49

Corrosion

The degradation of metals due to natural electrochemical processes is known as corrosion. Rust formation on iron, tarnishing of silver, and the blue-green patina that develops on copper are examples of corrosion. Corrosion involves the oxidation of metals. Sometimes it is protective, such as the oxidation of copper or aluminum, wherein a protective layer of metal oxide or its derivatives forms on the surface, protecting the underlying metal from further oxidation. In other cases, corrosion is...
25.6K
Mixtures of Acids03:27

Mixtures of Acids

The pH of a solution containing an acid can be determined using its acid dissociation constant and its initial concentration. If a solution contains two different acids, then its pH can be determined using one of several methods depending upon the relative strength of the acids and their dissociation constants.
A Mixture of a Strong Acid and a Weak Acid
In a mixture of a strong acid and a weak acid, the strong acid dissociates completely and becomes a source of almost all the hydronium ions...
20.1K
Acid Attack on Concrete01:21

Acid Attack on Concrete

When acids come into contact with concrete, they initiate a chemical reaction that dissolves the hydrated cement paste. This process leads to softening and structural weakening of the concrete. This issue is commonly observed in environments such as chimneys, sewers, and industrial settings. The severity of the damage increases as the pH of the water interacting with the concrete drops below 6.5. In particular, a pH under 4.5 can cause significant concrete damage.
The rate at which hydrogen...
347
Sample Preparation for Analysis: Advanced Techniques01:08

Sample Preparation for Analysis: Advanced Techniques

Accurate analysis of complex samples often requires advanced preparation techniques to achieve reliable and reproducible results. Samples containing inorganic or organic materials can be challenging to dissolve or decompose effectively. Standard sample preparation methods include acid digestion, fusion, dry ashing, and wet digestion.
Acid digestion with strong acids is commonly used to dissolve inorganic materials that are insoluble (do not dissolve) in water. This method can be useful for...
472
Polyprotic Acids03:38

Polyprotic Acids

Acids are classified by the number of protons per molecule that they can give up in a reaction. Acids such as HCl, HNO3, and HCN that contain one ionizable hydrogen atom in each molecule are called monoprotic acids. Their reactions with water are: