Ni-Al-Cr superalloy as high temperature cathode current collector for advanced thin film Li batteries

Alejandro N Filippin1, Tzu-Ying Lin1, Michael Rawlence1

  • 1Laboratory for Thin Films and Photovoltaics, Empa - Swiss Federal Laboratories for Materials Science and Technology Überlandstrasse 129, CH-8600 Dübendorf Switzerland nico.qca@gmail.com Stephan.Buecheler@empa.ch.