Impact of Atomization Pressure on the Particle Size of Nickel-Based Superalloy Powders by Numerical Simulation
Yongquan Qing1,2,3, Kuaikuai Guo1,2, Chen Liu1,2
1School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China.
Abstract:
Vacuum induction melting gas atomization (VIGA) has evolved as an important production technique of superalloy powders used in additive manufacturing. However, the development of powder preparation techniques is limited because the crushing process of gas-atomized metal melt is difficult to characterize by conventional experimental methods. Herein, we report the application of computational fluid dynamics to simulate the breaking behavior of droplets in the process of preparing nickel-based superalloy powders by VIGA, as well as the results on the effect of gas pressure on the atomization process and powder particle size distribution of metal melt. In the process of primary atomization, the crushing morphology of superalloy melt shows an alternate transformation of umbrella shapes and inverted mushroom cloud shapes, and with the increase in atomization pressure, the disorder of the two-phase flow field increases, which is conducive to sufficient breakage of the melt. Most importantly, in the process of secondary atomization and with the increasing atomization pressure, the particle size distribution becomes narrower, the median particle diameter and average particle size decrease, and the decreasing trend of the particle size increases gradually. The simulation results are compliant with the performed nickel-based superalloy powder preparation tests. This study provides insight into the production and process optimization of superalloy powder prepared by the VIGA method.