Abstract:
Three-point bending test, compression test and tensile test can detect the mechanical properties of the whole layer of skull, but cannot detect the mechanical properties of the inner plate, the diploe and the outer plate of the skull. In this study, nanoindentation technology was applied to detect mechanical properties of micro-materials of the skull, and differences in micro-mechanical properties of the inner, diploe and outer plates of the skull and cranial suture of human carcasses at different ages were analyzed. The differences in hardness (HIT) and modulus of elasticity (E) were statistically significant among different age groups (P < 0.01). In terms of structure, the E of diploe was higher than that of other structures, while HIT had no significant statistical difference. In terms of location, both HIT and E showed that left frontal (LF) was significantly higher than coronal suture (CS). The above results were consistent with the multi-factor ANOVAs. In addition, the multi-factor ANOVAs further explained the interaction of HIT and E with age, location and structure. It was believed that the nanoindentation technique could be used to analyze laws of micromechanical properties of different structures of human cadaveric skull and cranial suture.