Bond Behavior of FRP Bars in Lightweight SCC under Direct Pull-Out Conditions: Experimental and Numerical
Mohammed A Abed1, Zaher Alkurdi2, Jan Fořt3
1John A. Reif, Jr. Department of Civil and Environmental Engineering, New Jersey Institute of Technology, Newark, NJ 07102, USA.
Abstract:
In recent decades, lightweight aggregate concrete (LWC) became a popular building material due to its desired properties. However, various attributes of LWC, such as bond behavior of used reinforcing, have not been described thoroughly. In this regard, LWC produced with 0%, 50%, and 100% expanded clay aggregate was designed, and the physical-mechanical properties were assessed for material characterization. Subsequently, the bond behaviors of LWC reinforced with steel, glass fiber reinforced polymer (GFRP), and basalt fiber reinforced polymer (BFRP) bars were evaluated by pull-out tests. The results of the experimental program allowed the effects of expanded clay aggregate incorporation on LWC properties to be quantified. The bond strength of BFRP bars was not affected by the replacement of coarse aggregate by expanded clay aggregate, whilst the GFRP bars showed lower bond strength values of LWC specimens. Contrarily, in the case of steel bars, both the bond strength and bond stiffness were higher for LWC specimens than for those of normal concrete. Finite element software ATENA 3D was used for simulation of the bond behavior of LWC, and the model validated by the experimental results referred to reasonably corresponding outputs.
Related Concept Videos
Fiber Reinforced Concrete
Behavior of Concrete Under Compressive Load
As the concrete specimen fractures under...
Reinforcements in Concrete
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Impact Strength of Concrete