Effect of HAc on the Metastable Pitting Corrosion of 304 SS in NaCl Solution

Hanlu Zhang1, Wenqiang Huang2, Han Wei2

  • 1No. 92228 of the People's Liberation Army, Beijing 100072, China.

Related Concept Videos

Corrosion of Reinforcement01:27

Corrosion of Reinforcement

The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
264
Complexation Equilibria: The Chelate Effect01:19

Complexation Equilibria: The Chelate Effect

In complexation reactions, metal atoms or cations interact with ligands to form donor-acceptor adducts called metal complexes. Ligands that bind through one donor site are monodentate, ligands with two donor sites are bidentate, and those with more than two donor sites are polydentate ligands. For example, ethylene diamine is a bidentate ligand that binds through two nitrogen donor atoms, forming a five-membered ring. EDTA is a polydentate ligand that binds through four oxygen and two nitrogen...
693
Ionic Strength: Effects on Chemical Equilibria01:19

Ionic Strength: Effects on Chemical Equilibria

The addition of an inert ionic compound increases the solubility of a sparingly soluble salt. For example, adding potassium nitrate to a saturated solution of calcium sulfate significantly enhances the solubility of calcium sulfate. Le Châtelier's principle cannot predict this shift in the equilibrium. Instead, this could be explained in terms of changes in the effective concentration of the ions in solution in the presence of added inert salt.
In this solution, the primary...
1.8K
Complexation Equilibria: Factors Influencing Stability of Complexes01:09

Complexation Equilibria: Factors Influencing Stability of Complexes

In complexation reactions, metal cations are the electron pair acceptors, and the ligands are the electron pair donors. The stability of the metal complexes depends primarily on the complexing ability of the central metal ion and the nature of the ligands. Generally, the complexing ability of the metal ion depends on the size and charge of the ion. As the metal ion size increases, the stability of the metal complexes decreases, provided that the valency of the metal ion and the ligands remain...
494
Ladder Diagrams: Complexation Equilibria01:07

Ladder Diagrams: Complexation Equilibria

Ladder diagrams are useful for evaluating equilibria involving metal-ligand complexes. The vertical scale of the ladder diagram represents the concentration of unreacted or free ligand, pL. The horizontal lines on the scale depict the log of stepwise formation constants for metal-ligand complexes and indicate the dominant species in all the regions.
The formation constant, K1, for the formation of Cd(NH3)2+ complex from cadmium and ammonia is 3.55 × 102. Log K1 (i.e. pNH3) is 2.55, and...
426
Calculating pH Changes in a Buffer Solution02:45

Calculating pH Changes in a Buffer Solution

A buffer can prevent a sudden drop or increase in the pH of a solution after the addition of a strong acid or base up to its buffering capacity; however, such addition of a strong acid or base does result in the slight pH change of the solution. The small pH change can be calculated by determining the resulting change in the concentration of buffer components, i.e., a weak acid and its conjugate base or vice versa. The concentrations obtained using these stoichiometric calculations can be used...
54.2K