A Computational Pitting Corrosion Model of Magnesium Alloys
Chia-Jung Chang1, Chih-Han Chang1, Tin-Kan Hung2
1Department of Biomedical Engineering, National Cheng Kung University, Tainan, Taiwan.
Abstract:
Controlling the corrosion rate of implants to maintain mechanical properties during tissue healing is significant in developing magnesium alloy implants. In addition to surface treatment and material properties, the study of geometric alteration and mechanical strength are also vital for implant development. In this study, we developed a three-dimensional model for semi-autonomous computational pitting corrosion. It is based on the Monte Carlo method, modeling magnesium alloy implants toward clinical application. The corrosion probability is based on the number of exposed surfaces to saline and the oxidation characteristics of the elements. The computational results are well compared with the experimental measurement using micro-computed tomography (micro-CT) in 500 h. Subsequently, the computational analysis is extended to 3,000 h of corrosion analysis. The 3D model appears promising to assist the development of biodegradable implants.
Related Concept Videos
Corrosion of Reinforcement
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
Corrosion
Temperature Dependent Deformation
Stresses under Combined Loadings
The process begins by slicing the tube at critical points and analyzing the internal forces and stress components at these sections, focusing on the centroid. Normal stresses, generated by axial forces and bending moments, are either compressive or tensile and vary across the section from...