Pore Structure Characteristics and Strength Variation of Red Sandstone under Freeze-Thaw Cycles

Yongwei Lan1, Hongmei Gao2, Yanlin Zhao2

  • 1College of Mining Engineering, Heilongjiang University of Science and Technology, Harbin 150022, China.

Related Concept Videos

Frost Action on Concrete01:27

Frost Action on Concrete

Concrete structures in cold climates, such as those along roadsides, can retain moisture. This moisture makes them susceptible to frost-related damage when temperatures fall below freezing. Adding moisture worsens the damage during temperature fluctuations, leading to repeated freezing and thawing. De-icing salts, spread over these structures to melt ice, add to the freeze-thaw cycle, and draw even more moisture into the concrete.
This freeze-thaw cycle primarily causes surface scaling, where...
152
Pore Size Distribution01:23

Pore Size Distribution

In concrete, the pore size distribution significantly influences the material's properties. Capillary pores, markedly larger than gel pores, form a vast network within partially hydrated cement paste, reducing the concrete's strength and increasing its permeability. This heightened permeability leads to a greater risk of damage from environmental factors like freeze-thaw cycles and chemical attacks, with the extent of vulnerability also being tied to the water-to-cement ratio.
Adequate...
222
Unsoundness of Aggregate due to Volume Change01:26

Unsoundness of Aggregate due to Volume Change

Unsoundness in aggregates due to volume changes is primarily caused by the physical alterations aggregates undergo, such as freezing and thawing, thermal changes, and wetting and drying. Unsound aggregates, when subjected to these changes, result in volume change upon disintegration. This, in turn, contributes to the deterioration of concrete, including scaling, pop-outs, and cracking. Particular types of aggregates, such as porous flints, cherts, and those containing clay minerals, are...
186
Frost Resistant Concrete01:29

Frost Resistant Concrete

Concrete's susceptibility to frost damage during freeze-thaw cycles demands strategic measures to enhance its frost resistance. Employing techniques like air entrainment, adjusting the water-cement ratio, proper curing, and selecting appropriate aggregates are essential.
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
142
Brick Durability, Strength, and Appearance01:15

Brick Durability, Strength, and Appearance

Brick durability, strength, and appearance are crucial factors in construction, influencing the choice of bricks for specific applications. The process of freeze-thaw, for instance, significantly affects brick durability. This phenomenon occurs when water absorbed by a brick expands as it freezes, potentially causing damage when it melts and refreezes. Bricks are graded for durability: SW-grade bricks are the most durable, offering high strength and low water absorption, followed by MW-grade...
394
Mortar Joint Deterioration in Masonry01:13

Mortar Joint Deterioration in Masonry

Mortar joint deterioration is a significant concern in masonry structures, with water accumulation in the joints leading to damage from freeze-thaw cycles. The repeated expansion of water during freezing and its melting during thawing develop and propagate cracks in the masonry joints. Eventually, this leads to the spalling of mortar from the joints, loosening masonry units and weakening the structure. The deteriorated mortar joints are also vulnerable to moisture intrusion into the walls.
The...
166