Microstructural Effects in the Development of Near-Neutral pH Stress Corrosion Cracks in Pipelines
Ci Zhang1, Minrui Ran1, Yao Wang2
1National Center for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083, China.
Abstract:
The corrosion and stress corrosion cracking (SCC) behaviors of 20#, X60, and X80 pipeline steels in a near-neutral pH environment were investigated by means of electrochemical measurement, immersion test, and interrupted slow strain rate tensile (SSRT) test. The propensity for SCC, as indicated by the stress threshold value for crack initiation, was found to be dependent on the type of steel microstructure. Cracks were initiated in the high-strength steel X80 at a stress less than its yield strength, whereas in the other lower-grade steels, the initiation of cracks occurred after the yielding point. The threshold stress of SCC initiation in the near-neutral pH environment for 20#, X60, and X80 steels were 130.64% σys, 106.79% σys, and 86.92% σys, respectively. The SCC of 20# and X60 were characterized by the formation of transgranular and intergranular cracks, while X80 steel was only by transgranular cracking. The occurrence of corrosion had a great effect on crack initiation and the growth at the later stage. The latter involved hydrogen effects. A correlation between SCC sensitivity and the yield strength of the steel has been identified.
Related Concept Videos
Microcracking in Concrete
Types of Non-structural Cracks in Concrete
Plastic shrinkage cracks typically form within hours after the concrete is poured. The concrete's surface dries faster than the bottom, creating tensile stress that the still-plastic concrete cannot withstand, leading to diagonal or randomly patterned cracks on the concrete surface.
Corrosion of Reinforcement
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
Stresses under Combined Loadings
The process begins by slicing the tube at critical points and analyzing the internal forces and stress components at these sections, focusing on the centroid. Normal stresses, generated by axial forces and bending moments, are either compressive or tensile and vary across the section from...
Stress Concentrations
Residual Stresses