Related Experiment Video
Updated: Aug 5, 2026

Molecular Entanglement and Electrospinnability of Biopolymers
Published on: September 3, 2014
A Review: Current Status and Emerging Developments on Natural Polymer-Based Electrospun Fibers
Weisen Han1, Liangyu Wang1, Qin Li1
1Beijing Laboratory of Biomedical Materials, Beijing University of Chemical Technology, Beijing, 100029, P. R. China.
Abstract:
In recent years, natural polymer-based electrospun fibers (EFs) with huge specific surface area, good biocompatibility, and biological activity obtained from electrospinning process exhibit tremendous vitality in the field of biomedical areas. Herein, the parameters of electrospinning from two perspectives, polymer solution such as solvent, polymeric relative molecular mass, concentration, viscosity, and conductivity of the solution, and electrospinning process such as spinning voltage, spinning flow rate, needle tip to collector distance, temperature, and humidity are first detailed. Next, the raw materials consisting of polysaccharides such as cellulose, hyaluronic acid, alginate, and chitosan as well as proteins such as collagen, gelatin, silk fibroin, and keratin are summarized. The preparation method and related characteristics of EFs with multistage structures such as porous, core-shell, Janus, bamboo-like and other structures are introduced. The biomedical applications of these natural polymer-based EFs mainly including tissue engineering, drug sustained release, wound dressings, and biomedical sensors are systematically recapitulated. Finally, the outlook on natural EFs is further proposed.
More Related Videos
12:21Fabrication and Characterization of Griffithsin-modified Fiber Scaffolds for Prevention of Sexually Transmitted Infections
Published on: October 31, 2017
08:28Vapor Phase Deposition of Electroactive Poly(3,4-ethylenedioxythiophene) onto Electrospun Commodity Polymer Nanofibers
Published on: March 7, 2025
Related Concept Videos
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...
Classification and Mechanical Properties of Synthetic Polymers