Bacterial Performance in Crack Healing and its Role in Creating Sustainable Construction

Digafe Alemu1,2, Wubetie Demiss1,2, Gamachis Korsa1,2

  • 1Center of Excellence for Biotechnology and Bioprocess, Addis Ababa Science and Technology University, P.O. Box 16417, Addis Ababa, Ethiopia.

Related Concept Videos

Waterproofing and Anti-Bacterial Admixtures in Concrete01:22

Waterproofing and Anti-Bacterial Admixtures in Concrete

Concrete's susceptibility to water absorption is due to the capillary action within the pores of its hydrated cement paste. This action draws water in, creating the need for waterproofing admixtures to prevent such penetration. The efficacy of these admixtures is contingent upon the water pressure, with variations arising from different conditions such as rain, capillary rise, or hydrostatic pressure in structures intended to hold water.
Waterproofing admixtures render concrete hydrophobic,...
111
Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
202
Bacterial Signaling01:30

Bacterial Signaling

Bacterial signaling can occur within bacteria (intracellular) or between bacteria (intercellular). At times, a group of bacteria behaves like a community. To achieve this, they engage in quorum sensing, the perception of higher cell density that causes changes in gene expression. Quorum sensing involves both extracellular and intracellular signaling. The signaling cascade starts with a molecule called an autoinducer (AI). Individual bacteria produce AIs that move out of the bacterial cell...
33.9K
Types of Non-structural Cracks in Concrete01:28

Types of Non-structural Cracks in Concrete

Non-structural cracks are primarily of three types: plastic, early-age thermal, and drying shrinkage cracks. Plastic cracks are further classified into plastic shrinkage cracks and plastic settlement cracks.
Plastic shrinkage cracks typically form within hours after the concrete is poured. The concrete's surface dries faster than the bottom, creating tensile stress that the still-plastic concrete cannot withstand, leading to diagonal or randomly patterned cracks on the concrete surface.
243
Curing of Concrete01:20

Curing of Concrete

The hydration of cement takes place within the water-filled capillary pores. However, environmental elements can disrupt this process by evaporating water from the concrete surfaces. Sealed concrete with a water-cement ratio below 0.5 experiences self-desiccation, leading to water loss. The water loss in concrete is mitigated by curing. This technique involves keeping the concrete saturated to maintain the necessary temperature and moisture conditions, to optimally fill the spaces in the cement...
163
Types of Cement I01:21

Types of Cement I

Portland cement comes in several types, each with distinct properties and applications based on their chemical composition and hydration characteristics:
Type I (Ordinary Portland Cement) is widely used for general construction where special properties are not required. It has moderate sulfate resistance and heat of hydration.
Type II (Modified Cement) offers moderate resistance to sulfate attack and a lower rate of heat development compared to Type I. It is suitable for structures in...