Designed for Molecular Recycling: A Lignin-Derived Semi-aromatic Biobased Polymer
Published on: November 30, 2020
Bio-Based Degradable Poly(ether-ester)s from Melt-Polymerization of Aromatic Ester and Ether Diols
Lesly Dasilva Wandji Djouonkep1,2,3,4, Alain Pierre Tchameni1,2,3, Naomie Beolle Songwe Selabi5
1College of Petroleum Engineering, Applied Chemistry in Oil and Gas Fields, Yangtze University, Wuhan 430100, China.
Abstract:
Vanillin, as a promising aromatic aldehyde, possesses worthy structural and bioactive properties useful in the design of novel sustainable polymeric materials. Its versatility and structural similarity to terephthalic acid (TPA) can lead to materials with properties similar to conventional poly(ethylene terephthalate) (PET). In this perspective, a symmetrical dimethylated dialkoxydivanillic diester monomer (DEMV) derived from vanillin was synthesized via a direct-coupling method. Then, a series of poly(ether-ester)s were synthesized via melt-polymerization incorporating mixtures of phenyl/phenyloxy diols (with hydroxyl side-chains in the 1,2-, 1,3- and 1,4-positions) and a cyclic diol, 1,4-cyclohexanedimethanol (CHDM). The polymers obtained had high molecular weights (Mw = 5.3-7.9 × 104 g.mol-1) and polydispersity index (Đ) values of 1.54-2.88. Thermal analysis showed the polymers are semi-crystalline materials with melting temperatures of 204-240 °C, and tunable glass transition temperatures (Tg) of 98-120 °C. Their 5% decomposition temperature (Td,5%) varied from 430-315 °C, which endows the polymers with a broad processing window, owing to their rigid phenyl rings and trans-CHDM groups. These poly(ether-ester)s displayed remarkable impact strength and satisfactory gas barrier properties, due to the insertion of the cyclic alkyl chain moieties. Ultimately, the synergistic influence of the ester and ether bonds provided better control over the behavior and mechanism of in vitro degradation under passive and enzymatic incubation for 90 days. Regarding the morphology, scanning electron microscopy (SEM) imaging confirmed considerable surface degradation in the polymer matrices of both polymer series, with weight losses reaching up to 35% in enzymatic degradation, which demonstrates the significant influence of ether bonds for biodegradation.
More Related Videos
12:07Fabricating Degradable Thermoresponsive Hydrogels on Multiple Length Scales via Reactive Extrusion, Microfluidics, Self-assembly, and Electrospinning
Published on: April 16, 2018
08:12Depolymerizable Olefinic Polymers Based on Fused-Ring Cyclooctene Monomers
Published on: December 16, 2022
Related Concept Videos
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the...
Olefin Metathesis Polymerization: Acyclic Diene Metathesis (ADMET)
Similar to cross-metathesis, ADMET also involves the formation of metallacyclobutane intermediate by [2+2] cycloaddition of one of the double bonds of a terminal diene with...
Free-Radical Chain Reaction and Polymerization of Alkenes
Olefin Metathesis Polymerization: Overview
Ruthenium-based Grubbs catalyst is the most commonly used catalyst for olefin metathesis polymerization. Grubbs catalyst consists...
Polymer Classification: Architecture
Olefin Metathesis Polymerization: Ring-Opening Metathesis Polymerization (ROMP)