Abstract:
At present, the many domestic, large mined-out areas caused by single filling ability of the slurry flow state, thin layer flow and hardening after filling in multilayer structure generally need to finish filling for many times, because after a filling experience shows that filling body in the last solidification of flow, this leads to a lower one side of the roof, and far distance part of the filling body cannot pick up top. The determination of backfill strength is the key problem of the cemented backfill method, and it is affected by many factors. Therefore, through theoretical calculation, laboratory testing and numerical simulation methods, combined with the field filling process, this paper has verified the flow accumulation and stratification characteristics of stope layered filling slurry. When the slurry concentration is 60−73%, the slope increases exponentially from 2.5° to 8°. It is revealed that the delamination and meshing state are the key factors to determine the overall strength of large-scale stope filling through the testing of particle size distribution in interlayer and flow direction. The reduction effect of the number and Angle of structural weak surface formed by layering and filling on strength is revealed: cement−sand ratio 1:12, concentration 68%, standard curing R28 > 1.81 MPa. The strength reduction coefficient is 61.31% and 92.96% when the number of layers is 1−4. The higher the number of layers, the greater is the reduction coefficient, and when the stratification angle increases by 2, the strength of backfill decreases by 20−30%. The verification of stope filling coring shows that the in situ strength reaches 2.42 MPa, which is 0.61 MPa higher than the standard curing strength, with an increase of 33.7%. When the depth is from 1 m to 5 m, the strength increases from 2.26 MPa to 2.69 MPa, with an increase rate of 18.2%. Finally, through the research and application of the comprehensive technology of mining and filling coordination under the complex goaf group, the residual ore resources of Xianglushan tungsten mine are effectively recovered, the volume of goaf is significantly reduced, and the safety of goaf is improved.
More Related Videos
06:26Experimental Implementation of a New Composite Fabrication Method: Exposing Bare Fibers on the Composite Surface by the Soft Layer Method
Published on: October 6, 2017
08:26Development of Amelogenin-chitosan Hydrogel for In Vitro Enamel Regrowth with a Dense Interface
Published on: July 10, 2014
Related Concept Videos
Additives and Fillers in Concrete
The...
Porosity in Cement Paste
The balance of water to cement in the mix is...
Waterproofing and Anti-Bacterial Admixtures in Concrete
Waterproofing admixtures render concrete hydrophobic,...
Cavity Drainage and Flashings in Masonry walls
Weep holes, strategically placed at the base of the cavity, are critical for draining accumulated water. These openings are created by leaving head...
Masonry Cavity Walls
Maintaining a clean cavity during construction...