Compressive Strength Properties Perpendicular to the Grain of Hollow Glue-Laminated Timber Elements
Nikola Perković1, Jure Barbalić1, Vlatka Rajčić1
1Structural Department, Faculty of Civil Engineering, University of Zagreb, 10000 Zagreb, Croatia.
Abstract:
Timber is one of the fundamental materials of human civilization, it is very useful and ecologically acceptable in its natural environment, and it fits very well with modern trends in green construction. The paper presents innovative hollow glued laminated (GL) timber elements intended for log-house construction. Due to the lack of data on the behavior of the hollow timber section in compression perpendicular to the grain, the paper presented involves testing the compression strength of elliptical hollow cross-section glue-laminated timber specimens made of softwood and hardwood, as well as full cross-section glue-laminated softwood timber specimens. The experimental research was carried out on a total of 120 specimens. With the maximal reduction of 26% compared to the full cross-section, regardless of the type of wood and direction of load, the compression strength perpendicular to the grain of hollow specimens decreases by about 55% compared to the full cross-section, with the coefficient kc,90 equal to 1.0. For load actions at the edge and the middle of the element, kc,90 factors were obtained with a value closer to those obtained for full cross-section, which indicates the same phenomenology, regardless of cross-sectional weakening. At the same time, the factors in the stronger axis are lower by about 10%, and in the weaker axis by about 30% compared to those prescribed by the Eurocode. Experimental research was confirmed by FEM analysis. Comparative finite element analysis was performed in order to provide recommendations for future research and, consequently, to determine the optimal cross-section form of the hollow GL timber element. By removing the holes in the central part of the cross-section, the stress is reduced. The distance of the holes from the edges defines the local cracking. Finally, if the holes are present only in the central part of the element, the behavior of the element is more favorable.
Related Concept Videos
Structural Properties and Dimensions of Lumber
The strength characteristics of...
Wood Products
Glue-laminated wood, often referred to as glulam, combines multiple smaller pieces of dimensional lumber using adhesives to form a single, larger piece. Cross-laminated timber consists...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Relation Between Tensile Strength and Compressive Strength of Concrete
Prismatic Beams: Problem Solving
The design begins with analyzing the beam as a free body to identify moments and force balances, thereby determining support reactions. Next, the...
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen...