A sequential leaching procedure for efficient recovery of gold and silver from waste mobile phone printed circuit
Zhi-Yuan Zhang1, Lixiang Wu1, Kai He1
1Department of Solid Waste Treatment and Recycling, Research Center for Eco-Environmental Sciences, Chinese Academy of Sciences, Beijing 100085, China; University of Chinese Academy of Sciences, Beijing 100049, China.
Abstract:
The present study reports a sequential, non-acid process for effective recovery of copper and precious metals from mobile phone printed circuit boards. In this process, gold and silver were first enriched during the synthesis process of cuprous chloride and then leached by thiosulfate method. Results indicated that the distribution of gold and silver in the liquid and solid phases during the synthesis of cuprous chloride process was affected by the [Cu]/[Cu2+] ratio. Enrichment of gold and silver in the residue after the cuprous chloride synthesis could be achieved by the adjusting the [Cu]/[Cu2+] ratio. The silver and gold leaching rates of the residue after cuprous chloride synthesis (93.8 % silver and 99 % gold) were much higher than those of the raw PCB sample (27.0 % silver and 14.2 % gold) under the same conditions. This process has the advantages of high leaching efficiency, high leaching rate and avoiding the use of HNO3 or aqua regia commonly used for copper, gold and silver recovery. Thus, this study offers a promising and environmentally friendly method for recovering valuable metals from e-waste.
Related Concept Videos
Washing, Drying, and Ignition of Precipitates
Extraction: Advanced Methods
Electrodeposition
Electrodeposition can...