Failure behavior of coated nickel-based superalloy under thermomechanical fatigue
Abstract:
Thermomechanical fatigue (TMF) is a major life limiting factor for gas turbine blades. In this study, the failure behavior of NiCrAlY overlay coated nickel-based superalloy M963 was investigated under out of phase (OP) TMF. All tests were carried out under mechanical strain control with a cyclic period of 200 s. Results revealed that the fatigue life of high velocity oxygen fuel spraying (HVOF) coated specimen was longer than that of air plasma spraying (APS) coated one, but shorter than that of bare superalloy M963 at a given strain range. It was found that cracking process in the APS coating was different from that in the HVOF coating, which was shown by the sketches to understand the crack initiation and propagation behavior.
More Related Videos
09:35Applying Dynamic Strain on Thin Oxide Films Immobilized on a Pseudoelastic Nickel-Titanium Alloy
Published on: July 28, 2020
14:51An Available Technique for Preparation of New Cast MnCuNiFeZnAl Alloy with Superior Damping Capacity and High Service Temperature
Published on: September 23, 2018
Related Concept Videos
Fatigue
Yield Criteria for Ductile Materials under Plane Stress
The Maximum Shearing Stress Criterion, also known as...
Stress-Strain Diagram - Ductile Materials
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Plastic Behavior