Conformal atomic layer deposition of RuOon highly porous current collectors for micro-supercapacitor applications
Related Experiment Video
Updated: Jun 29, 2026

Atomically Defined Templates for Epitaxial Growth of Complex Oxide Thin Films
Published on: December 4, 2014
Sakeb Hasan Choudhury1, Guillaume Vignaud2, Pascal Dubreuil1
1LAAS-CNRS, Université de Toulouse, CNRS, 7 avenue du colonel Roche, F-31400 Toulouse, France.
Abstract:
3D porous electrodes have been considered as a new paradigm shift for increasing the energy storage of pseudocapacitive micro-supercapacitors for on-chip electronics. However, the conformal deposition of active materials is still challenging when highly porous structures are involved. In this work, we have investigated the atomic layer deposition (ALD) of ruthenium dioxide RuO2on porous Au and Pt architectures prepared by hydrogen bubble templated electrodeposition, with area enlargement factors ranging from 400 to 10 000 cm2/cm2. Using proper ALD conditions, a uniform RuO2coverage has been successfully obtained on porous Au, with a specific electrode capacitance of 8.1 mF cm-2and a specific power of 160 mW cm-2for a minute amount of active material. This study also shows the importance of the chemical composition and reactivity of the porous substrate for achieving conformal deposition of a ruthenium oxide layer.
More Related Videos
08:50Fabrication and Characterization of a Conformal Skin-like Electronic System for Quantitative, Cutaneous Wound Management
Published on: September 2, 2015
08:14Improved Heterojunction Quality in Cu2O-based Solar Cells Through the Optimization of Atmospheric Pressure Spatial Atomic Layer Deposited Zn1-xMgxO
Published on: July 31, 2016
Related Concept Videos
Capacitor With A Dielectric
Dielectrics are non-conducting materials with no free or loosely bound electrons. When a dielectric is...
MOS Capacitor
The metal gate is typically made from highly conductive materials such as aluminum or polysilicon. Beneath the metal gate lies a thin layer of...