Related Experiment Video
Updated: Aug 28, 2025

Key Factors Affecting the Performance of Sb2S3-sensitized Solar Cells During an Sb2S3 Deposition via SbCl3-thiourea Complex Solution-processing
Published on: July 16, 2018
Numerical Simulation of the Performance of Sb2Se3 Solar Cell via Optimizing the Optoelectronic Properties Based
Shahbaz Abbas1, Saraswati Bajgai1, Shahariar Chowdhury1
1Faculty of Environmental Management, Prince of Songkla University, Hat Yai, Songkhla 90110, Thailand.
Abstract:
Antimony trisulfide (Sb2Se3), a non-toxic and accessible substance, has possibilities as a material for use in solar cells. The current study numerically analyses Sb2Se3 solar cells through the program Solar Cell Capacitance Simulator (SCAPS). A detailed simulation and analysis of the influence of the Sb2Se3 layer's thickness, defect density, band gap, energy level, and carrier concentration on the devices' performance are carried out. The results indicate that a good device performance is guaranteed with the following values in the Sb2Se3 layer: an 800 optimal thickness for the Sb2Se3 absorber; less than 1015 cm-3 for the absorber defect density; a 1.2 eV optimum band gap; a 0.1 eV energy level (above the valence band); and a 1014 cm-3 carrier concentration. The highest efficiency of 30% can be attained following optimization of diverse parameters. The simulation outcomes offer beneficial insights and directions for designing and engineering Sb2Se3 solar cells.