A two-step approach for calculating chloride diffusion coefficient in concrete with both natural and recycled

Wei-Bin Yuan1, Lixuan Mao2, Long-Yuan Li2

  • 1College of Architecture and Civil Engineering, Zhejiang University of Technology, Hangzhou 310023, China.

Related Concept Videos

Deleterious Substances in Aggregate01:25

Deleterious Substances in Aggregate

Deleterious substances in aggregates can be detrimental to the quality and durability of concrete. These substances include organic impurities like loam, which interfere with cement hydration and are usually present in the sand. These prevent a good bond between aggregate and cement paste. Organic impurities can be detected using the colorimetric test, where the darkness of a solution after agitation indicates the level of organic content.
Another type of impurity is clay and fine material that...
232
Aggregate Cement Ratio01:21

Aggregate Cement Ratio

The Aggregate Cement ratio refers to the weight of aggregate divided by the weight of cement in a concrete mix. Altering this ratio has profound effects on the concrete's properties. This ratio plays a pivotal role in determining the strength, workability, and durability of concrete. When the Aggregate Cement ratio is higher, the mix is leaner, meaning it has less cement paste to lubricate the aggregate, potentially making the concrete less workable. Such mixes, known as lean, enhance the...
303
Design Example: Aggregate Gradation01:24

Design Example: Aggregate Gradation

The right type and quality of aggregates are crucial for concrete as they significantly influence its properties, mix proportions, and cost-effectiveness. If different sources are available for sand, the commonly used fine aggregate in concrete, the selection of sand is primarily based on its gradation.
The grading, or particle-size distribution, of sand is determined using sieve analysis, with standard sizes ranging from 150 μm to 10 mm (ASTM No. 100 sieve to 3⁄8 in. sieve). Sand is...
145
Alkali Aggregate Reaction in Concrete01:26

Alkali Aggregate Reaction in Concrete

The alkali-aggregate reaction in concrete involves natural siliceous minerals in aggregates reacting with alkaline hydroxides derived from cement alkalis. This reaction forms an alkali-silica gel that absorbs water, swells, and increases in volume, which is confined by the surrounding cement paste, creating internal pressures that crack and disrupt the concrete. The extent of expansion and damage can be partly attributed to the alkali-silica reaction's osmotic hydraulic pressure and the...
172
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
168
Segregation in Fresh Concrete01:16

Segregation in Fresh Concrete

Segregation in fresh concrete is a phenomenon where the components of the concrete mix separate, leading to uneven distribution and compromised structural integrity. This separation typically occurs when concrete is subjected to excessive horizontal movement within forms, or when it is dropped from considerable heights or forced through narrow, winding paths. As a result, heavier coarse aggregate particles settle at the bottom, while lighter, finer materials such as cement and water rise to the...