Effect of Exposure to Environmental Cycling on the Thermal Conductivity of Expanded Polystyrene
Sergiu George Petre1, Dorina Nicolina Isopescu1, Marian Pruteanu1
1Department of Civil and Industrial Engineering, "Gheorghe Asachi" Technical University of Iasi-Romania, Blvd. Mangeron, No. 1, 700050 Iasi, Romania.
Abstract:
The global effort to reduce energy consumption generated by buildings involves the increasing use of thermal insulation materials, with expanded polystyrene representing one of the most used materials to this end. The thermal performance of expanded polystyrene has been extensively studied; however, information on the effect of exposure to cyclic environmental conditions on its thermal performance is limited. Therefore, we conducted such a study, which is presented in this article. In the first stage, samples were subjected to 28 days of preconditioning to accelerate the increase in moisture in the material. The second stage involved exposure to 40 freeze-thaw cycles of 12 h each. The weight and thermal conductivity of the samples were measured before and after exposure, and the compression behavior was also analyzed. The results show a decrease in the thermal performance of expanded polystyrene exposed to cyclic environmental conditions, as demonstrated by an increase in the water content of the material under the same measurement conditions and an increase of 5.06% in the average thermal conductivity. The influence of this increase on the thermal performance of commonly used wall construction elements was also been studied and presented in this article. A decrease of 7.59% in the compressive stress of the material at 10% strain was also demonstrated.
Related Concept Videos
Thermal Insulation in Masonry Walls
External insulation can be applied using an Exterior Insulation and Finish System (EIFS), which involves affixing panels of plastic foam to the wall and covering them with a polymeric stucco reinforced with glass fiber mesh....
Thermal Stress
Thermal Expansion
Thermal expansion and Thermal stress: Problem Solving
To solve the problem, first, identify the known and unknown quantities. The initial length (L) of the bridge is 1275 m, the coefficient of linear expansion (α) for steel is 12 x 10-6/°C, and the change in...
Conduction, Convection and Radiation: Problem Solving
In order to solve a problem related to heat transfer, first of all, the situation needs to be examined to determine the type of heat transfer involved. This could...
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...