Related Experiment Video
Updated: Aug 23, 2025

Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
The Influence of the Thickness of the Materials for the Provisionalization in Minimally Invasive Restorations
Ildefonso Serrano-Belmonte1, Nerea Roca-Cánovas1, Eva K Linares-Tovar1
1Faculty of Medicine, School of Dentistry, Clínica Odontológica Universitaria, Hospital Morales Meseguer, Universidad de Murcia, Avda. Marqués de los Vélez s/n, 30008 Murcia, Spain.
Abstract:
This in vitro study aimed to determine the flexural strength and modulus of elasticity of two bisacrylic resins for temporary crowns at different thicknesses, i.e., Structur 3 and Structur Premium, and to compare them with each other. Sixty samples were prepared, thirty of each material, which were made at different thicknesses (1 mm, 1.5 mm, and 2 mm). The dimensions followed the UNE-EN ISO 178:2019 standard, with a length of 24 mm, a width of 10 mm, and the thicknesses described. Materials were subjected to a three-point bending test. For the modulus of elasticity, statistically significant differences were observed between the 1.5 mm and 2 mm thicknesses of Structur 3 material. For Structur Premium, statistically significant differences were observed between the thicknesses 1 mm and 1.5 mm as well as between 1 mm and 2 mm thickness. With respect to flexural strength, no statistically significant differences were observed for either material at the different thicknesses. Significant differences were observed between the materials for both flexural strength and modulus of elasticity, being higher for Structur Premium: Structur Premium has a higher flexural strength and modulus of elasticity than Structur 3. There are significant differences for the modulus of elasticity but not for the flexural strength between thicknesses.